Galvanic Corrosion ?'s
Permalink  
 


I just finished painting my aluminum grill and was reading about the installation.  Originally the grill was held on by aluminum rivets.  I am going to use either a SS bolt or a plain steel  plated bolt.

 

I was reading about galvanic corrosion and it seem there will be some kind of corrosion between the aluminum grill and the bolt.  I was wondering if there was something I could do to eliminate or reduce the corrosion and which bolt would cause less corrosion?  Thanks



__________________

Jim L

Lake City



Founding Member

Status: Offline
Posts: 2861
Date:
Permalink  
 

I have seen thin clear plastic washers used to separate dissimilar materials... not sure where to get them though.

__________________

Derek Kiefer - Mantorville, MN

69 Malibu Pro-Touring stroker LS1-383/T56 - 69 SS396-325/3spd project



2K+ Club

Status: Offline
Posts: 2447
Date:
Permalink  
 

Nylon nuts, bolts and washer can be found at any good hardware store, Home Depot and Lowes have them. I was going to suggest nylon bolts or fasteners.

__________________

Kevin

Northwestern Ohio



President

Status: Offline
Posts: 7432
Date:
Permalink  
 

All I use is clear packaging tape. It only takes a film of insulation to prevent the galvanic reaction. I used the tape under the mirrors and lights on the Pete, as all the brackets were SS and the cab was aluminum.



__________________

Mitch D.   River Falls, WI

Lifetime member of the "Cars apart Club"

1966 Chevelle SS 396 M20

1970 Chevelle SS 396 M20

1967 Camaro SS/RS 350 M20



2K+ Club

Status: Offline
Posts: 2447
Date:
Permalink  
 

If it't excessive you may want to check your grounds, adding current through those parts will accelerate the galvanic reaction.

__________________

Kevin

Northwestern Ohio



2K+ Club

Status: Offline
Posts: 2786
Date:
Permalink  
 

It not a big problem as I replaced some screw headed bolts about 9 years ago with a flat headed bolt and there seems to be little or no reaction.  I just thought if there was something easy to try I would do that.  Thanks, probable with look for some thin nylon washers, like those used on some bolts and washers  on   my doors and strikers or just the packaging tape.

 

So Kevin, if you have good grounds, then the process is reduced?



__________________

Jim L

Lake City



2K+ Club

Status: Offline
Posts: 2820
Date:
Permalink  
 

I'm running a salvage/scrounged (300% better than what was in him) grille assy in Blackie that I pulled from a yard.

I dunked it in a lye solution to remove the anodizing, and spent a few zillion hours one winter smoothing the 40+ years of sandblast and dents. Another 1/2 zillion hours with various buffing wheels and compounds and I've got a really nice polished grille. It's not re-anodized or cleared... I just hit it with some "Blue Magic" polish occasionally.

I remounted it using stainless 10-32 allen button-heads and nylock nuts. It's been there 7+ years and ZERO reaction so far.

__________________

 

John D. - St. Louis Park, MN.

1965 El Camino - LT-1, 4L60e, 4wh discs, SC&C susp.
2013 F-150 Platinum - Twin Turbo 3.5

2018 Factory Five MkIV Roadster build thread



2K+ Club

Status: Offline
Posts: 2447
Date:
Permalink  
 

jim larson wrote:

So Kevin, if you have good grounds, then the process is reduced?


 I think it will help, at the very least it won't be accelerated by other means. I also believe poor grounds will accelerate corrosion and mineral deposits in your radiator as the water becomes a partial conductor.   



__________________

Kevin

Northwestern Ohio